I got my Lee molds from F&M Reloading, but they are slow as mollases in January, I don't think they keep stock, but the prices are good.... I got a Lee Production Pot IV (10 lb. pot, bottom pour, 4" clearance under, which you need for the hollowpoint conversions I bought (also from F&M).... I use a pea-sized piece of (local) beeswax for fluxing, but I'm starting with pure lead ingots, not junk lead, so very little is required.... BUY A THERMOMETER !!!!!!!!!!!!
If you want hollowpoint molds, just order the Lee, already converted, from Erik, I think they are $79.... One you definitely want is the 113 gr. Lee FN 0.309", I think it would be GREAT with a HP conversion.... I also have a Lee press and sizing dies (I have a 0.308").... and some Hornady sizing lube for the die....
Bob




Reply With Quote